ASTM A519 mechanical tubing

ASTM A519 specification covers for several grades of carbon and alloy steel mechanical tubing, either hot-finished or cold-finished.

Application:
For mechanical engineering
For mechanical and pressure use,and also for transporting steam,water,gas and etc.

Size range(mm):
Out diameter:10-324mm
Wall Tickness:1-30mm
Length:14000mm max

Main Grade of ASTM A519:

  • ASTM A519 1020
  • ASTM A519 1025
  • ASTM A519 1035
  • ASTM A519 1045
  • ASTM A519 4130
  • ASTM A519 4140

Note:
DN — Nominal Diameter
NPS —Nominal Pipe Size

Pipe and Tube Specifications

This specification covers for several grades of carbon and alloy steel mechanical tubing, either hot-finished or cold-finished. The steel used in the mechanical tubing may be cast in ingots or may be strand cast. When steel of different grades is sequentially strand cast, identification of the resultant transition material is required. The seamless tubing is a tubular product made without a welded seam. It is usually manufactured by hot working steel, and if necessary, by subsequently cold finishing the hot-worked tubular product to produce the desired shape, dimensions and properties. The tubes shall be furnished in the following shapes: round, square, rectangular and special sections. Heat analysis shall be made to determine the percentages of the elements specified. If secondary melting processes are used, the heat analysis shall be obtained from one remelted ingot or the product of one remelted ingot of each primary melt. The tubing shall be coated with a film of oil before shaping to retard rust when specified This abstract is a brief summary of the referenced standard. It is informational only and not an official part of the standard; the full text of the standard itself must be referred to for its use and application. ASTM does not give any warranty express or implied or make any representation that the contents of this abstract are accurate, complete or up to date.

Steel ASTM A519 Grade and Chemical composition (%)
Grade C Mn P≤ S≤ Si Cr Mo
1008 ≤0.10 0.30-0.50 0.040 0.050
1010 0.08-0.13 0.30-0.60 0.040 0.050
1018 0.15-0.20 0.60-0.90 0.040 0.050
1020 0.18-0.23 0.30-0.60 0.040 0.050
1025 0.22-0.28 0.30-0.60 0.040 0.050
1026 0.22-0.28 0.60-0.90 0.040 0.050
4130 0.28-0.33 0.40-0.60 0.040 0.050 0.15-0.35 0.80-1.10 0.15-0.25
4140 0.38-0.43 0.75-1.00 0.040 0.050 0.15-0.35 0.80-1.10 0.15-0.25
Mechanical Properties
Grade Condition MPa Tenslle Point Yield Point Elongation
1020 CW ≥414 ≥483 ≥5%
SR ≥345 ≥448 ≥10%
A ≥193 ≥331 ≥30%
N ≥234 ≥379 ≥22%
1025 CW ≥448 ≥517 ≥5%
SR ≥379 ≥483 ≥8%
A ≥207 ≥365 ≥25%
N ≥248 ≥379 ≥22%
4130 SR ≥586 ≥724 ≥10%
A ≥379 ≥517 ≥30%
N ≥414 ≥621 ≥20%
4140 SR ≥689 ≥855 ≥10%
A ≥414 ≥552 ≥25%
N ≥621 ≥855 ≥20%

Please note the meaning of below abbreviation in table 2:

  • HR—-Hot Rolled
  • CW—-Cold Worked
  • SR—-Stress Relieved
  • A—-Annealed
  • N—-Normalized
Dimension Tolerances
Pipe Type Pipe Sizes Tolerances
Cold Drawn OD ≤48.3mm ±0.40mm
WT ≥60.3mm ±1%mm

— Tech & service —

ASTM A519-89/ASME SA519 Standard specification

ASTM A519- specification covers for several grades of carbon and alloy steel mechanical tubing, either hot-finished or cold-finished.

  • ASTM A213 T11 Seamless alloy pipe
    ASTM A213 T11 Standard covers seamless ferritic and austenitic steel boiler, superheater, and heat-exchanger tubes.